Material: High Strength Polymeric Tubing with hot melt adhesive Shrink Ratio: Exceeds 3 to 1 Minimum Shrink Temperature: 90° C Continuous Operating Temperature: -55° C to 125° C Flammability: Non-flame retardant Concentricity: 70%
Physical
Test Method
Performance
Tensile Strength
ASTM D2671
3,770 psi
Elongation:
ASTM D2671
500%
Longitudinal Change:
ASTM D2671
1% to -10%
Specific Gravity:
ASTM D729
0.96
Heat Resistance:
ASTM D2671 (158°C / 168 hrs)
No cracking, flowing, or dripping of outer wall
Heat Shock:
ASTM D2671 (225°C / 4 hrs)
No cracking, flowing, or dripping of outer wall
Low Temperature Flexibility:
ASTM D2671 (-55°C / 1 hr)
No cracking or splitting of outer wall
Electrical
Test Method
Performance
Dielectric Strength:
ASTM D2671
500V/mil (20kV/mm)
Chemical
Test Method
Performance
Fluid Resistances*:
ASTM D2671
Good
Copper Corrosion:
ASTM D2671
Not Corrosive
Water Absorbtion:
ASTM D570
0.5% Max